64 Mbit SPI Quad I/O NOR flash — the 80 MHz read speed and 1.7 V rail
The S25FS064SDSNFN030: At 125 °C ambient, the flash's data retention and read current derate per the datasheet profile — a factor when sizing the thermal budget in a sealed enclosure.
8-LGA package — what the rework bench needs to know
Pin 1 is marked by a chamfer on the package corner — visible under a 10× loupe after reflow. The LGA's flat bottom wicks solder evenly if the pad design has a 1:1 solder-mask-defined opening; a solder-mask-defined pad with a smaller aperture risks head-in-pillow joints on the centre pads.
Sourced through authorized and independent distribution; availability and pricing confirmed at RFQ.